Tech specs:
- Blade rotating speed: 25~35m/sec
- cutting depth: 20~40mm/time
- Blade quantity per set: 30~35pcs (dia.1200mm)
- Blade diameter: dia.1200mm
- Segment size: 24 x 6.5/7.5 x 12mm
- Segment No.: 80pcs
- Tested in Iran by: Kimiya Gohar Vazin, Baharavaran
- Recommed: First cut hard granite then cut soft granite for better
segment sharpening result.
Tested and approved by:
1, Baharavaran (Iran)
2, S.V.Diamond (India)
Bond choice as per the table below:
| type |
STDP 01
(grade 1) |
STDP 02
(grade 2) |
STDP 03
(grade 3) |
STDP 04
(grade 4) |
| Fast cutting |
|
|
|
|
| Normal |
|
QGW-02-001D
moving speed: 1.8~2.0m/min
Life: 220~280sqm |
|
HGW-04-001D
moving speed:2.8~3.0m/min
Life: 350~400sqm |
| Long life |
JWGW-01-001DB
moving speed: 1.8~2.0m/min
Life: 250~300sqm |
|
|
QGW-04-001DB
moving speed:2.0~2.2m/min
Life: 500~700sqm |
* Cutting performance may be different against actual application, all
information above only from the cutting in laboratory in RobtoL &
RobLion.
update: Dec.31, 2009 |